岩土力学 ›› 2021, Vol. 42 ›› Issue (4): 1115-1125.doi: 10.16285/j.rsm.2020.1336

• 基础理论与实验研究 • 上一篇    下一篇

不同预制裂缝方法及长度对岩石三点弯曲 试验的影响

卢浩1, 2,冯夏庭1, 3,杨成祥3,张希巍3   

  1. 1. 中国科学院武汉岩土力学研究所 岩土力学与工程国家重点实验室,湖北 武汉 430071;2. 中国科学院大学,北京 100049; 3. 东北大学 深部金属矿山安全开采教育部重点实验室,辽宁 沈阳 110819
  • 收稿日期:2020-09-04 修回日期:2020-11-02 出版日期:2021-04-12 发布日期:2021-04-26
  • 通讯作者: 张希巍,男,1976年生,博士,教授,主要从事试验岩石力学方面的研究。E-mail: zhangxiwei@mail.neu.edu.cn E-mail:luhaosc@foxmail.com
  • 作者简介:卢浩,男,1996年生,硕士研究生,主要从事岩石三点弯曲试验方面的研究
  • 基金资助:
    国家重点研发计划(No. 2018YFC0407006)

Effect of different notch prefabrication methods and notch lengths on rock three-point bending test

LU Hao1, 2, FENG Xia-ting1, 3, YANG Cheng-xiang3, ZHANG Xi-wei3   

  1. 1. State Key Laboratory of Geomechanics and Geotechnical Engineering, Institute of Rock and Soil Mechanics, Chinese Academy of Sciences, Wuhan, Hubei 430071, China; 2. University of Chinese Academy of Sciences, Beijing 100049, China; 3. Key Laboratory of Ministry of Education on Safe Mining of Deep Metal Mines, Northeastern University, Shenyang, Liaoning 110819, China
  • Received:2020-09-04 Revised:2020-11-02 Online:2021-04-12 Published:2021-04-26
  • Supported by:
    This work was supported by the National Key Research and Development Program of China (2018YFC0407006).

摘要: 为选择岩石三点弯曲试验合适的预制裂缝方法和裂缝长度以获得相对准确可靠的岩石I型断裂韧度KIC,并了解岩石三点弯曲宏观断裂过程和细观断裂特征,采用线切割、锯片切割和水刀切割3种方法预制花岗岩和大理岩三点弯曲梁试样直切槽裂缝,以研究不同预制裂缝方法对岩石KIC的影响,结合场发射扫描电镜比较了不同切割方法岩样的细观断裂特征,试验结果表明线切割方法对岩石KIC测试结果的影响最小。另对含无量纲裂缝长度0.1、0.2、0.3、0.4和0.5的花岗岩及大理岩试样进行试验测得岩石KIC随裂缝长度增加呈先增大后减小的趋势,建议使用? =0.3的裂缝长度进行试验以得到有代表性的岩石KIC值。岩样破坏宏观上经历变形局部化带萌生、局部化带发展、裂纹起裂、最终扩展断裂的过程,声发射过程显示岩样破坏的脆性特征明显,裂缝开口位移与声发射累计曲线趋势一致,可视为试样内部破坏发展过程的宏观表征。

关键词: 岩石三点弯曲试验, I型断裂韧度, 预制裂缝方法, 裂缝长度, 断裂过程

Abstract: To select an appropriate notch prefabrication method and notch length for obtaining relatively accurate and reliable rock mode I fracture toughness (KIC), as well as to improve understanding on macro fracture process and meso-fracture characteristics in the rock three-point bending test, three methods, i.e., wire cutting, saw blade cutting and water jet cutting were used to prefabricate notch in granite and marble specimens for three-point bending test. The comparison of micro fracture characteristics among three different cutting methods was conducted with the application of scanning electronic microscopic. The test results show that the effect of wire cutting method on KIC is the smallest. In addition, three-point bending tests on granite and marble containing dimensionless notch length of 0.1, 0.2, 0.3, 0.4, and 0.5 show that KIC tends to increase firstly and then decrease with increasing notch length. The dimensionless notch length of ? =0.3 is recommended for obtaining the representative KIC. The macroscopic failure of rock specimen undergoes a process of initiation of localization zone, development of localization zone, crack initiation, and finally fracture propagation. The acoustic emission process of rock specimen is observed with an obvious brittle characteristic, the crack opening displacement curve is consistent with the trend of cumulative acoustic emission curve, and the evolution of crack opening displacement curve can be regarded as a macroscopic characterization of the specimen internal failure development process.

Key words: rock three-point bending test, mode I fracture toughness, notch prefabrication method, notch length, fracture process

中图分类号: 

  • TU 452
[1] 曹虎, 张广清, 李世远, 汪文瑞, 谢彭旭, 孙伟, 李帅, . 基于断裂过程区的压裂驱油水力裂缝 扩展模型及应用[J]. 岩土力学, 2025, 46(3): 798-810.
[2] 汪文瑞, 张广清, 孙伟, 李帅, 曹虎, 李祖亮, . 岩性差异对裂缝穿层扩展的率相关断裂特征影响[J]. 岩土力学, 2024, 45(8): 2311-2323.
[3] 陈磊, 张广清, 张敏, 曹庾杰, 谌立吉, . 水力裂缝穿越非连续面扩展时的断裂过程研究[J]. 岩土力学, 2023, 44(1): 159-170.
[4] 吴顺川, 孙伟, 刘洋, 成子桥, 许学良, . Ⅰ型断裂韧度模拟方法及细观影响因素研究[J]. 岩土力学, 2020, 41(8): 2536-2546.
[5] 张 盛, 王龙飞, 常 旭, 王东坤, 王小良, 乔 洋, . 中心直裂纹半圆盘试样的石灰岩断裂韧度 尺寸效应试验研究[J]. 岩土力学, 2019, 40(5): 1740-1749.
[6] 赵子江,刘大安,崔振东,唐铁吾,韩伟歌,. 半圆盘三点弯曲法测定页岩断裂韧度(KIC) 的实验研究[J]. , 2018, 39(S1): 258-266.
[7] 郭俊志,谢其泰,王建力,. 边缘裂缝圆盘砂岩试体III型断裂韧度量测之研究[J]. , 2016, 37(S1): 263-266.
[8] 袁会娜,张 骏,张其光. 掺砾黏土拉伸断裂细观特性研究[J]. , 2016, 37(11): 3096-3104.
[9] 刘冬梅 ,宋超业 ,陈志勇 . 钢纤维混凝土断裂过程激光实时全息干涉法研究[J]. , 2007, 28(9): 1997-2002.
Viewed
Full text


Abstract

Cited

  Shared   
  Discussed   
No Suggested Reading articles found!