酸性干湿循环作用下砂岩强度参数劣化规律

傅 晏1,2,袁 文3,刘新荣4,5,缪露莉4,谢文博4   

  1. 1. 重庆大学 建设管理与房地产学院,重庆 400045;2. 重庆大学 建设经济与管理中心,重庆 400045;3. 深圳市建筑工务署,广东 深圳 518000;4. 重庆大学 土木工程学院,重庆 400045;5. 重庆大学 山地城镇建设与新技术教育部重点实验室,重庆 400045
  • 收稿日期:2016-11-19 出版日期:2018-09-11 发布日期:2018-10-08
  • 通讯作者: 袁文,男,1987年生,博士,主要从事工程管理方面的工作。E-mail:yuanwen_yyan@163.com E-mail:fuyan1981@foxmail.com
  • 作者简介:傅晏,男,1981年生,博士,副教授,主要从事岩土工程、工程管理方面的研究工作。
  • 基金资助:

    国家自然科学青年基金项目(No. 51308567);中央高校基本科研业务费(No. 106112017CDJXY030012)。

Deterioration rules of strength parameters of sandstone under cyclical wetting and drying in acid-based environment

FU Yan1, 2, YUAN Wen3, LIU Xin-rong4, 5, MIAO Lou-li4, XIE Wen-bo4   

  1. 1. Faculty of Construction Management and Real Estate, Chongqing University, Chongqing 400045, China; 2. Center for Construction Economics and Management, Chongqing University, Chongqing 400045, China; 3. Bureau of Public Works of Shenzhen Municipality, Shenzhen, Guandong 518000, China; 4. College of Civil Engineering, Chongqing University, Chongqing 400045, China; 5. Key Laboratory of New Technology for Construction of Cities in Mountain Area of Ministry of Education, Chongqing University, Chongqing 400045, China
  • Received:2016-11-19 Online:2018-09-11 Published:2018-10-08
  • Supported by:

    This work was supported by the Young Foundation of the National Natural Science Foundation of China(51308567) and the Fundamental Research Funds for the Central Universities(106112017CDJXY030012).

摘要: 为研究酸性环境中砂岩在干湿循环作用下强度的劣化规律,在溶液pH值分别为7、5、3的浸泡环境中,对砂岩试样进行循环次数为1、5、10、15、20次的干湿循环试验。根据每个循环阶段后的强度数据,得到Mohr-Coulomb强度准则参数和Hoek-Brown强度准则参数,并对这些参数的干湿循环劣化效应做简要的分析。再根据应力空间中偏应力与强度准则参数的关系式,分别作出pH值为7、5、3的浸泡溶液作用下π平面上的破坏面随不同循环次数的变化图。结果表明:各准则参数随着干湿循环次数的增加呈下降趋势,循环次数较小时劣化较为严重,而后呈缓和趋势;pH值越低,劣化越严重,劣化效应由大至小依次为:单轴抗压强度、黏聚力、材料常数、内摩擦角;同一pH值浸泡环境中,循环次数较小时,π平面上的破坏曲线较为稀疏,循环次数越大,破坏曲线越密集;不同pH值浸泡环境中,pH越低,破坏曲面越小;偏应力与单轴抗压强度、黏聚力正相关,与材料常数、内摩擦角负相关。

关键词: 干湿循环;砂岩;劣化;&pi, 平面;破坏准则

Abstract: To investigate the deterioration rule and failure criterion of rock in the acid-based environment, experiments were conducted on sandstone specimens after 1, 5, 10, 15, and 20 times of wetting and drying cycles in the environment of pH=7, 5 and 3, respectively. By analysing uniaxial compressive strength (UCS) and triaxial compressive strength (TCS) after different cycles, the parameters of Mohr-Coulomb failure criterion and Hoek-Brown failure criterion were calculated, and the effect of wetting and drying cycles on these parameters is also analysed. Finally, according to the relationship formula between the deviatoric stress and the strength criterion parameters in the stress space, the failure envelopes changed with cycles in the π-plane were drawn under the action of solutions with pH values of 7, 5, and 3. The results show that the parameters of strength criterion decrease with the increase of cycle time, at the early stage of cycles, the deterioration is more significant, and then the deterioration is relatively low. The lower the pH value is, the more serious the deterioration is, and the degrees of deterioration effect from large to small are as follow UCS, cohesion, material constant and internal friction angle. In the same environment of pH value, when the cycle number is low, the failure envelopes in the π-plane are relatively sparse. However, the greater the number of cycles are, the denser the failure envelope is; in the different immersion environment of pH value is, the lower the pH value is, the smaller the failure plane is. The deviatoric stress is positively correlated with UCS and cohesion, but negatively correlated with the material constant and internal friction angle.

Key words: wetting and drying, sandstone, deterioration, π-plane, failure criterion

中图分类号: 

  • TU 452

[1] 郭 亮,胡卸文,李晓昭,巫锡勇,吴礼舟,李 煜,罗 刚,马洪生,. 花岗岩断裂带原状裂隙岩水力特性试验研究[J]. , 2018, 39(11): 3937-3948.
[2] 张希巍,王 刚,蔡 明,徐 荃,. 凌海花岗岩变形特点与脆性评价[J]. , 2018, 39(10): 3515-3524.
[3] 陈 松,乔春生,叶 青,邓 斌. 基于摩尔-库仑准则的断续节理岩体复合损伤本构模型[J]. , 2018, 39(10): 3612-3622.
[4] 李术才,潘东东,许振浩,李利平,林 鹏,袁永才,高成路,路 为, . 承压型隐伏溶洞突水灾变演化过程模型试验[J]. , 2018, 39(9): 3164-3173.
[5] 左宇军,孙文吉斌,邬忠虎,许云飞,. 渗透压–应力耦合作用下页岩渗透性试验[J]. , 2018, 39(9): 3253-3260.
[6] 王凤云,钱德玲. 基于切向应变软化的深埋圆形隧道围岩弹塑性分析[J]. , 2018, 39(9): 3313-3320.
[7] 郑安兴,罗先启,. 危岩水力劈裂分析的扩展有限元法[J]. , 2018, 39(9): 3461-3468.
[8] 刘泉声,彭星新,黄 兴,雷广峰,魏 莱,刘 鹤,. 全断面隧道掘进机护盾受力监测及卡机预警[J]. , 2018, 39(9): 3406-3414.
[9] 李小飞,孙江涛,陈卫忠,袁敬强,刘金泉,张庆艳,. 纤维硅灰水泥石强度与浆液抗冲刷特性[J]. , 2018, 39(9): 3157-3163.
[10] 李东奇,李宗利,吕从聪. 考虑裂隙附加水压的岩体断裂强度分析[J]. , 2018, 39(9): 3174-3180.
[11] 吴永胜,谭忠盛,余贤斌,喻 渝,朱 勇,. 不同加载方位角下单轴压缩千枚岩扩容特性[J]. , 2018, 39(8): 2747-2754.
[12] 李 杨,佘成学. 堆石料单粒强度尺寸效应的颗粒流模拟方法研究[J]. , 2018, 39(8): 2951-2959.
[13] 李 帅,朱万成,牛雷雷,李如飞,李少华. 动态扰动对应力松弛岩石变形行为影响的试验研究[J]. , 2018, 39(8): 2795-2804.
[14] 王斐笠,王述红,修占国. 应力波扰动下结构面的应力量化及强度表征[J]. , 2018, 39(8): 2844-2850.
[15] 杨秀荣,姜谙男,江宗斌. 含水状态下软岩蠕变试验及损伤模型研究[J]. , 2018, 39(S1): 167-174.
Viewed
Full text


Abstract

Cited

  Shared   
  Discussed   
No Suggested Reading articles found!