岩土力学 ›› 2026, Vol. 47 ›› Issue (11): 3671-3685.doi: 10.16285/j.rsm.2025.1267CSTR: 32223.14.j.rsm.2025.1267

• 基础理论与实验研究 •    下一篇

全固废低碳固化剂固化赤泥的力学与环境稳定性演化机制

董晓强1, 2,崔雯雯1, 3,尹顺德3,李江山4,段伟1,王林浩1,薛生国5   

  1. 1. 太原理工大学 土木工程学院,山西 太原 030024;2. 太原科技大学 应用科学学院,山西 太原 030024; 3. 滑铁卢大学 土木与环境工程系,加拿大 滑铁卢市;4. 中国科学院武汉岩土力学研究所 岩土力学与工程安全全国重点实验室,湖北 武汉 430071;5. 中南大学 冶金与环境学院,湖南 长沙 410083
  • 收稿日期:2025-11-24 接受日期:2026-03-30 出版日期:2026-11-09 发布日期:2026-11-07
  • 通讯作者: 崔雯雯,女,2000年生,博士研究生,主要从事环境岩土方面的研究。E-mail: cuiwenwen0089@link.tyut.edu.cn
  • 作者简介:董晓强,男,1974年生,博士,教授,主要从事环境岩土等方面的研究。E-mail:dongxiaoqiang@tyut.edu.cn
  • 基金资助:
    国家自然科学基金(No. 52378360,No. 51978438);三晋英才计划科技创新领军人才项目(No. SJYC2025012);中国国家留学基金委资助(No. 202406930021);山西省研究生教育创新计划项目(No. 2025TD06)。

Evolution mechanisms of mechanical performance and environmental stability of red mud stabilized with an all-solid-waste, low-carbon binder

DONG Xiao-qiang1, 2, CUI Wen-wen1, 3, YIN Shun-de3, LI Jiang-shan4, DUAN Wei1, WANG Lin-hao1, XUE Sheng-guo5   

  1. 1. Department of Civil Engineering, Taiyuan University of Technology, Taiyuan, Shanxi 030024, China; 2. School of Applied Science, Taiyuan University of Science and Technology, Taiyuan, Shanxi 030024, China; 3. Department of Civil and Environmental Engineering, University of Waterloo, Waterloo, Canada; 4. State Key Laboratory of Geomechanics and Geotechnical Engineering Safety, Institute of Rock and Soil Mechanics, Chinese Academy of Sciences, Wuhan, Hubei 430071, China; 5. School of Metallurgy and Environment, Central South University, Changsha, Hunan 410083, China
  • Received:2025-11-24 Accepted:2026-03-30 Online:2026-11-09 Published:2026-11-07
  • Supported by:
    This work was supported by the National Natural Science Foundation of China (52378360, 51978438), the Science and Technology Innovation Leading Talent Project of the Sanjin Talents Program (SJYC2025012), the China Scholarship Council (202406930021) and the Graduate Education Innovation Program of Shanxi Province (2025TD06).

摘要:

赤泥是氧化铝工业产生的大宗固体废弃物,长期堆存易导致堆体强度低、稳定性不足等环境与工程风险,而传统水泥固化方法存在碳排放高、固稳效率受限等问题。以钢渣、粉煤灰和磷石膏等多源工业固废为原料,采用单纯形重心法优化配比,构建了一种用于赤泥加固的全固废低碳固化剂体系。研究结果表明,当赤泥、钢渣、粉煤灰和磷石膏质量比为 54:9:27:10时,体系可协同生成水化硅酸钙C-S-H(calcium silicate hydrate)、水化硅铝酸钙C-A-S-H(calcium aluminosilicate hydrate)和钙矾石Aft(ettringite)等水化产物,固化体90 d抗压强度达到约14 MPa,渗透系数为7.4×10⁻7 cm/s;固结不排水(consolidated undrained,简称CU)三轴试验获得的黏聚力约为13 kPa、内摩擦角约为30°,表明固化体强度与刚度得到明显提升。Na+固化率为63.5%,Pb、As和Cr等重金属的固化率均不低于75.0%,其浸出浓度均低于相应浸出毒性限值。经冻融-盐蚀耦合作用后,固化体质量损失率与强度衰减幅度均保持在较低水平,表现出良好的耐久性。研究结果可为赤泥堆场的原位加固与资源化利用提供低碳技术支撑。

关键词: 赤泥, 全固废低碳固化剂, 堆场加固, 污染物固稳, 耐久性

Abstract:

 Red mud, a bulk solid waste generated by the alumina industry, is commonly stockpiled for long periods, which can induce environmental and geotechnical risks such as low pile strength and insufficient stability. Conventional cement stabilization, however, is constrained by high carbon emissions and limited immobilization efficiency. In this study, a low-carbon, all-solid-waste binder system for red mud stabilization was developed using steel slag, fly ash, and phosphogypsum as multi-source industrial solid wastes, and the mix proportions were optimized via the simplex centroid method. Results show that at a red mud/steel slag/fly ash/phosphogypsum mass ratio of 54:9:27:10, the system synergistically forms hydration products including calcium silicate hydrate (C-S-H), calcium aluminosilicate hydrate (C-A-S-H), and ettringite (AFt). The stabilized material achieved a 90-day compressive strength of approximately 14 MPa and a hydraulic conductivity of 7.4×10⁻⁷ cm/s. Consolidated undrained (CU) triaxial tests yielded a cohesion of approximately 13 kPa and an internal friction angle of approximately 30°, indicating pronounced improvements in the strength and stiffness of the stabilized material. The immobilization efficiency of Na⁺ was 63.5%, and those of heavy metals such as Pb, As, and Cr were all no less than 75.0%, with leachate concentrations below the corresponding leaching toxicity limits. After coupled freeze–thaw and salt-erosion exposure, both mass loss and strength degradation remained low, demonstrating favorable durability. These findings provide a low-carbon technical basis for in situ stabilization and resource-oriented utilization of red mud stockpiles.

Key words: red mud, all-solid-waste low-carbon binder, stockpile reinforcement, pollutant immobilization, durability

中图分类号: TQ 172
[1] 卢正, 则志辉, 赵阳, 柴少强, 刘斌, 李元彪, 姚海林. 基于开挖弃土与粉煤灰的泡沫轻质土物理力学性能及耐久性分析[J]. 岩土力学, 2026, 47(6): 1917-1928.
[2] 常仕奇, 董晓强, 刘晓凤, 李江山, 刘晓勇, 张豪儒, 黄寅豪, . 水位变动引发干法赤泥堆场坝体失稳的模型试验与数值模拟研究[J]. 岩土力学, 2025, 46(4): 1122-1130.
[3] 崔雯雯, 董晓强, 刘晓勇, 赵睿阳, 贺高乐, 张蒙, 周磊, 武学文, . 赤泥基胶凝材料的水化动力学过程及其水化机制研究[J]. 岩土力学, 2025, 46(3): 867-880.
[4] 聂庆科, 张海清, 杨海朋, 贾向新, 张日华. 赤泥−粉煤灰地聚物桩的开发与现场试验研究[J]. 岩土力学, 2025, 46(12): 3683-3693.
[5] 李爽, 李江山, 张平, 刘磊, 杜月林, 朱磊, 高腾飞, 陈亿军, . 垃圾腐殖土固化回填可行性试验研究[J]. 岩土力学, 2024, 45(S1): 84-94.
[6] 李丽华, 方亚男, 肖衡林, 李文涛, 曹毓, 徐可, . 赤泥复合物固化/稳定化镉污染土特性研究[J]. 岩土力学, 2022, 43(S1): 193-202.
[7] 谈云志, 柯睿, 陈君廉, 吴军, 邓永锋. 偏高岭土增强石灰-水泥固化淤泥的耐久性研究[J]. 岩土力学, 2020, 41(4): 1146-1152.
[8] 和法国, 吕燃, 粟华忠, 周瑾, 张景科, 王南, . SH材料加固夯筑遗址土耐久性试验及机理研究[J]. 岩土力学, 2019, 40(S1): 297-307.
[9] 王东星, 肖杰, 李丽华, 肖衡林, . 基于碳化-固化技术的武汉东湖淤泥 耐久性演变微观机制[J]. 岩土力学, 2019, 40(8): 3045-3053.
[10] 王东星, 王宏伟, 邹维列, 徐学勇, . 活性MgO−粉煤灰固化淤泥耐久性研究[J]. 岩土力学, 2019, 40(12): 4675-4684.
[11] 陈瑞锋,田高源,米栋云,董晓强,. 赤泥改性黄土的基本工程性质研究[J]. , 2018, 39(S1): 89-97.
[12] 杨海朋,白 冰,聂庆科,. 赤泥渗沥液对黏性土和固化赤泥影响的试验研究[J]. , 2017, 38(S1): 299-304.
[13] 冯燕博 ,刘东燕 ,刘芳语 ,刘 伟 ,韩朦朦,. 混合赤泥胶结特性产生机制及对其力学特性的影响试验研究[J]. , 2016, 37(1): 49-56.
[14] 于博伟,杜延军,刘辰阳,薄煜琳. 活性MgO碱性激发粒化高炉矿渣固化黏土的抗硫酸盐侵蚀试验研究[J]. , 2015, 36(S2): 64-72.
[15] 刘 楷 ,李仁民 ,杜延军 ,魏明俐 , . 气泡混合轻质土干湿循环和硫酸钠耐久性试验研究[J]. , 2015, 36(S1): 362-366.
Viewed
Full text


Abstract

Cited

  Shared   
  Discussed   
No Suggested Reading articles found!