岩土力学 ›› 2019, Vol. 40 ›› Issue (5): 1740-1749.doi: 10.16285/j.rsm.2017.2555

• 基础理论与实验研究 • 上一篇    下一篇

中心直裂纹半圆盘试样的石灰岩断裂韧度 尺寸效应试验研究

张 盛1, 2,王龙飞1,常 旭3,王东坤1,王小良1,乔 洋1   

  1. 1. 河南理工大学 能源科学与工程学院,河南 焦作 454001;2. 河南理工大学 煤炭安全生产河南省协同创新中心,河南 焦作 454003; 3. 河南理工大学 土木与工程学院,河南 焦作 454001
  • 收稿日期:2017-12-25 出版日期:2019-05-11 发布日期:2019-06-02
  • 作者简介:张盛,男,1976年生,博士,教授,主要进行岩石断裂力学方面的研究
  • 基金资助:
    国家自然科学基金面上项目(No. 51674101);河南省重点实验室开放基金资助项目(No. S201605)。

Experimental study of size effect of fracture toughness of limestone using the notched semi-circular bend samples

ZHANG Sheng1, 2, WANG Long-fei1, CHANG Xu3, WANG Dong-kun1, WANG Xiao-liang1, QIAO Yang1   

  1. 1. School of Energy Science and Engineering, Henan Polytechnic University, Jiaozuo, Henan 454001, China; 2. Collaborative Innovation Center of Coal Work Safety, Henan Polytechnic University, Jiaozuo, Henan 454003, China; 3. School of Civil Engineering, Henan Polytechnic University, Jiaozuo, Henan 454001, China
  • Received:2017-12-25 Online:2019-05-11 Published:2019-06-02
  • Supported by:
    This work was supported by the National natural Science Foundation of China (51674101) and the State Key Laboratory Program of Henan Province (S201605).

摘要: 为了考察试样尺寸和预制裂缝长度对岩石断裂韧度测试值的影响,采用4种圆盘半径分别为25.0、37.5、50.0、 75.0 mm,预制裂缝长度与圆盘试样半径比值(无量纲裂缝长度)在0.3~0.7范围内的中心直裂纹半圆盘石灰岩试样(NSCB)进行了三点弯曲断裂试验。结果表明:NSCB试样的破坏过程表现出明显的“脆性”破坏特征。与预制裂缝长度相比,试样尺寸对峰值载荷和载荷-位移曲线的形态影响更显著;随着试样尺寸的增加,试样的断裂韧度测试值不断增加,增加幅度随着预制裂缝长度的增加而加剧;当试样尺寸一定时,随着无量纲裂缝长度的增加,断裂韧度测试值有一定程度降低;为减小尺寸效应的影响,建议采用圆盘半径大于37.5 mm,无量纲预制裂缝长度范围在0.4~0.6内的NSCB试样测试岩石的断裂韧度。所得结果为推广NSCB试样国际建议方法及准确测试岩石的断裂韧度提供了一定的参考。

关键词: 预制裂缝长度, 试样尺寸, 岩石断裂韧度, 中心直裂纹半圆盘试样(NSCB)

Abstract: This study is aimed to investigate the effects of the specimen size and prefabricated crack length on the rock fracture toughness. Then three-point bending tests are conducted on semi-circular limestone specimens (NSCB) with four disc radii of 25.0, 37.5, 50.0 and 75.0 mm, respectively. The ratio of prefabricated crack length to the radius of disc specimens (dimensionless crack length) ranged from 0.3 to 0.7. The results show that the failure process of NSCB specimens exhibits the characteristic of an obvious brittle failure. Compared with the prefabricated crack length, the specimen size has more significant influence on the peak load and the shape of load-deformation curve. As the specimen size increases, the testing values of fracture toughness increase continuously. Moreover, the increase rate increases with the length of the prefabricated crack length. For a selected-size specimen, the testing value of fracture toughness reduces with the increase of prefabricated crack length. In order to reduce the effect of size effect in the fracture toughness test, it is suggested that the radius of NSCB specimen is greater than 37.5 mm and the dimensionless prefabricated crack length is in the range of 0.4~0.6. This study provides certain references for the promotion of the international method and the accurate test of rock fracture toughness using NSCB specimens.

Key words: prefabricated crack length, specimen size, rock fracture toughness, notched semi-circular bend (NSCB)

中图分类号: 

  • TU 452
[1] 周 辉, 黄 磊, 姜 玥, 卢景景, 张传庆, 胡大伟, 李 震, . 岩石空心圆柱扭剪仪研制的重点问题及研究进展[J]. 岩土力学, 2018, 39(12): 4295-4304.
[2] 崔振东,刘大安,安光明,周 苗,李志清. V形切槽巴西圆盘法测定岩石断裂韧度KIC的实验研究[J]. , 2010, 31(9): 2743-2748.
[3] 张 盛,王启智. 用5种圆盘试件的劈裂试验确定岩石断裂韧度[J]. , 2009, 30(1): 12-18.
[4] 吴礼舟,贾学明,王启智. CCNBD断裂韧度试样的SIF新公式和在尺度律分析中的应用[J]. , 2004, 25(2): 233-237.
Viewed
Full text


Abstract

Cited

  Shared   
  Discussed   
No Suggested Reading articles found!