›› 2017, Vol. 38 ›› Issue (7): 1894-1902.doi: 10.16285/j.rsm.2017.07.007

• 基础理论与实验研究 • 上一篇    下一篇

干湿循环下黄土强度衰减与结构强度试验研究

袁志辉1,倪万魁2,唐 春1,胡盛明1,甘建军1   

  1. 1. 南昌工程学院 水利与生态学院,江西 南昌 330099;2. 长安大学 地质工程与测绘学院,陕西 西安 710054
  • 收稿日期:2016-07-28 出版日期:2017-07-10 发布日期:2018-06-05
  • 作者简介:袁志辉,男,1983年生,博士,讲师,主要从事岩土体稳定性方面的研究工作。
  • 基金资助:

    国家科技支撑计划课题(No.2013BAJ06B04);陕西省科技统筹创新工程计划项目(No.2012KTDZD03-04)。

Experimental study of structure strength and strength attenuation of loess under wetting-drying cycle

YUAN Zhi-hui1, NI Wan-kui2, TANG Chun1, HU Sheng-ming1, GAN Jian-jun1   

  1. 1. College of Water Conservancy and Ecological Engineering, Nanchang Institute of Technology, Nanchang, Jiangxi 330099, China; 2. College of Geology Engineerging and Geomatics, Chang′an University, Xi′an, Shaanxi 710054, China
  • Received:2016-07-28 Online:2017-07-10 Published:2018-06-05
  • Supported by:

    This work was supported by the National Key Research and Development Program of the Ministry of Science and Technology of China (2013BAJ06B04) and Co-Innovative Engineering Program of Science and Technology of Shaanxi Province, China (2012KTDZD03-04).

摘要: 针对干湿循环作用下黄土强度问题,系统地开展了常规三轴试验,提出了黄土结构强度和衰减强度的求取方法,探讨了不同围压和含水率对结构和衰减强度的影响,研究了黄土结构与衰减强度的关系。研究结果表明,黄土结构和衰减强度都随含水率的增大而减小,且呈良好的对数函数关系;结构和衰减强度都随围压的增大而增大,具有良好的线性关系;通过对结构和衰减强度的研究,发现多次干湿循环后原状黄土的强度衰减值与相应的重塑黄土的强度衰减值和黄土的结构强度之和基本相等,证明多次的干湿循环作用不仅仅打破了原状黄土的结构强度,并最终使得其与重塑黄土具有基本相同的土体结构。

关键词: 干湿循环, 黄土, 三轴试验, 结构强度, 衰减强度

Abstract: In this study, conventional triaxial tests were conducted to systematically investigate the strength characteristics of loess under the conditions of drying-wetting cycles. We proposed the methods for calculating structural strength and decay intensity of loess, and then discussed the effects of confining pressure and water content on structural strength and decay intensity. The relationship between structural strength and decay intensity was studied as well. The results show that the structural strength and decay intensity decrease with increasing water content and reveal a good logarithmic function with water content. The structural strength and decay intensity increase with the increase of confining pressure, which had a good linear function. The attenuated strength value of undisturbed loess after several drying-wetting cycles is almost equal to the sum of attenuated strength value of remolded loess and structural strength. It is proved that the action of the wetting-drying cycle not only broke the original structure of undisturbed loess, but also made the undisturbed and remolded loess have the same structure of soil mass.

Key words: wetting-drying cycle, loess, conventional triaxial test, structural strength, decay strength

中图分类号: 

  • TU 411.3

[1] 孟庆彬, 王杰, 韩立军, 孙稳, 乔卫国, 王刚, . 极弱胶结岩石物理力学特性及本构模型研究[J]. 岩土力学, 2020, 41(S1): 19-29.
[2] 郑方, 邵生俊, 佘芳涛, 袁浩, . 重塑黄土在不同基质吸力下的真三轴剪切试验[J]. 岩土力学, 2020, 41(S1): 156-162.
[3] 褚峰, 张宏刚, 邵生俊, 邓国华. 人工合成类废布料纤维纱加筋黄土力学变形性质及抗溅蚀特性试验研究[J]. 岩土力学, 2020, 41(S1): 394-403.
[4] 李丽华, 余肖婷, 肖衡林, 马强, 刘一鸣, 杨 星, . 稻壳灰加筋土力学性能研究[J]. 岩土力学, 2020, 41(7): 2168-2178.
[5] 杨志浩, 岳祖润, 冯怀平, . 非饱和粉土路基内水分迁移规律试验研究[J]. 岩土力学, 2020, 41(7): 2241-2251.
[6] 张磊, 海维深, 甘浩, 曹卫平, 王铁行, . 水平与上拔组合荷载下柔性单桩 承载特性试验研究[J]. 岩土力学, 2020, 41(7): 2261-2270.
[7] 王康宇, 庄妍, 耿雪玉, . 铁路路基粗粒土填料临界动应力试验研究[J]. 岩土力学, 2020, 41(6): 1865-1873.
[8] 温馨, 胡志平, 张勋, 柴少波, 吕新波, . 基于Green-Ampt模型的饱和−非饱和黄土入渗 改进模型及其参数研究[J]. 岩土力学, 2020, 41(6): 1991-2000.
[9] 方瑾瑾, 冯以鑫, 余永强, 李震, 林志斌, . 真三轴条件下的原状黄土增湿变形特性[J]. 岩土力学, 2020, 41(4): 1235-1246.
[10] 刘华, 何江涛, 赵茜, 王铁行, 郭超翊, . 酸污染原状黄土渗透微观特征演变规律试验研究[J]. 岩土力学, 2020, 41(3): 765-772.
[11] 张宗堂, 高文华, 张志敏, 唐骁宇, 邬俊, . 基于Weibull分布的红砂岩颗粒崩解破碎演化规律[J]. 岩土力学, 2020, 41(3): 877-885.
[12] 方瑾瑾, 冯以鑫, 王立平, 余永强, . 真三轴条件下非饱和黄土的有效应力屈服特性[J]. 岩土力学, 2020, 41(2): 492-500.
[13] 梁珂, 陈国兴, 刘抗, 王彦臻, . 饱和珊瑚砂最大动剪切模量的 循环加载衰退特性及预测模型[J]. 岩土力学, 2020, 41(2): 601-611.
[14] 程昊, 唐辉明, 吴琼, 雷国平. 一种考虑水力滞回效应的非饱和土弹塑性扩展 剑桥本构模型显式算法有限元实现[J]. 岩土力学, 2020, 41(2): 676-686.
[15] 梁珂, 何杨, 陈国兴, . 南沙珊瑚砂的动剪切模量和阻尼比特性试验研究[J]. 岩土力学, 2020, 41(1): 23-31.
Viewed
Full text


Abstract

Cited

  Shared   
  Discussed   
No Suggested Reading articles found!